MODIFIED CONJUGATED DIENE POLYMER, BALE, METHOD FOR PRODUCING MODIFIED CONJUGATED DIENE POLYMER, RUBBER COMPOSITION, AND TIRE

DRIVE June 10, 2026
Source
A modified conjugated diene-based polymer, satisfying the following to : a Mooney viscosity measured at 100°C is 100 or more and 180 or less; a Mooney stress relaxation measured at 100°C is in a range of 0.10 to 0.40; a glass transition temperature is -95°C to -45°C; a content of silicon atoms is 100 ppm by mass or more with respect to a total amount of the modified conjugated diene-based polymer; a content of nitrogen atoms is 50 ppm by mass or more with respect to a total amount of the modified conjugated diene-based polymer; and a content of an antioxidant is 0.5 parts by mass or less with respect to 100 parts by mass of the modified conjugated diene-based polymer.