"$type": "site.standard.document",
"description": "Provided is a separator that includes a matrix including a polyolefin having a weight average molecular weight (M) of 250,000 to 450,000 and a molecular weight distribution (M/M) of 3 to 7; and a silane-modified polyolefin crosslinked in the matrix, and a method of manufacturing the same.",
"path": "/patents/1255814",
"publishedAt": "2020-02-27T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M2/1653",
"W-SCOPE KOREA CO., LTD."
],
"textContent": "Provided is a separator that includes a matrix including a polyolefin having a weight average molecular weight (M) of 250,000 to 450,000 and a molecular weight distribution (M/M) of 3 to 7; and a silane-modified polyolefin crosslinked in the matrix, and a method of manufacturing the same.",