  "$type": "site.standard.document",
  "description": "A method of preparing a positive electrode active material for a secondary battery includes preparing a positive electrode active material precursor including nickel (Ni), cobalt (Co), and at least one selected from the group consisting of manganese (Mn) and aluminum (Al); and forming a lithium…",
  "path": "/patents/1270239",
  "publishedAt": "2020-08-20T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/525",
    "LG Chem, Ltd."
  ],
  "textContent": "A method of preparing a positive electrode active material for a secondary battery includes preparing a positive electrode active material precursor including nickel (Ni), cobalt (Co), and at least one selected from the group consisting of manganese (Mn) and aluminum (Al); and forming a lithium composite transition metal oxide by mixing the positive electrode active material precursor and a lithium source and performing calcination, wherein the positive electrode active material precursor includes nickel (Ni) in an amount of 60 mol % or more out of the entire metal element, and a molar ratio (Li/M) of lithium (Li) of the lithium source to the entire metal element (M) of the positive electrode active material precursor is greater than 1.1.",
  "title": "Method of Preparing Positive Electrode Active Material for Secondary Battery"
}