  "$type": "site.standard.document",
  "description": "A method for manufacturing an electrode for an all solid battery including the steps of coating a current collector with a slurry including an active material, a conductive material, and a polyimide-based binder; and melting a solid electrolyte having a melting temperature of 50° C. to 500° C. and…",
  "path": "/patents/1274115",
  "publishedAt": "2020-10-08T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/0404",
    "LG CHEM, LTD."
  ],
  "textContent": "A method for manufacturing an electrode for an all solid battery including the steps of coating a current collector with a slurry including an active material, a conductive material, and a polyimide-based binder; and melting a solid electrolyte having a melting temperature of 50° C. to 500° C. and applying it onto the coating layer and an electrode manufactured therefrom.",
  "title": "ELECTRODE FOR SOLID-STATE BATTERY AND MANUFACTURING METHOD THEREFOR"
}