"description": "The present invention relates to a method for pre-lithiation of a negative electrode for a secondary battery, for reducing the time required for pre-lithiation and reducing changes in volume of the electrode. The present invention comprises an electrolyte wetting step of immersing a negative…",
"path": "/patents/1433263",
"publishedAt": "2023-10-18T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/052",
"LG CHEMICAL LTD [KR]"
],
"textContent": "The present invention relates to a method for pre-lithiation of a negative electrode for a secondary battery, for reducing the time required for pre-lithiation and reducing changes in volume of the electrode. The present invention comprises an electrolyte wetting step of immersing a negative electrode for a secondary battery in the electrolyte, and a pre-lithiation step of pre-lithiating the negative electrode, wherein the electrolyte wetting step includes a step of introducing the prepared negative electrode into an electrolyte bath containing the electrolyte, and a vacuum application step of removing bubbles and moisture in the negative electrode by applying a vacuum to the electrolyte bath in which the negative electrode is immersed.",
"title": "METHOD FOR PRE-LITHIATION OF NEGATIVE ELECTRODE FOR SECONDARY BATTERY"
}