"$type": "site.standard.document",
"description": "A method for producing a sulfide solid electrolyte having an argyrodite-type crystal structure may involve: mixing a raw material containing elemental phosphorus at an integrated power of 0.5 kWh/kg or more, and heat-treating a precursor obtained in the mixing at 350 to 500° C.",
"path": "/patents/1280830",
"publishedAt": "2021-01-07T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/0562",
"IDEMITSU KOSAN CO., LTD."
],
"textContent": "A method for producing a sulfide solid electrolyte having an argyrodite-type crystal structure may involve: mixing a raw material containing elemental phosphorus at an integrated power of 0.5 kWh/kg or more, and heat-treating a precursor obtained in the mixing at 350 to 500° C.",
"title": "METHOD FOR PRODUCING SULFIDE SOLID ELECTROLYTE HAVING ARGYRODITE-TYPE CRYSTAL STRUCTURE"
}