  "description": "The ultrahigh-molecular-weight polyethylene powder of the present invention is an ultrahigh-molecular-weight polyethylene powder having a viscosity-average molecular weight Mv of 10×10or higher and 1000×10or lower, wherein viscosity-average molecular weight Mv(A) of a kneaded product obtained by…",
  "path": "/patents/1281636",
  "publishedAt": "2021-01-21T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C08L23/06",
    "Asahi Kasei Kabushiki Kaisha"
  ],
  "textContent": "The ultrahigh-molecular-weight polyethylene powder of the present invention is an ultrahigh-molecular-weight polyethylene powder having a viscosity-average molecular weight Mv of 10×10or higher and 1000×10or lower, wherein viscosity-average molecular weight Mv(A) of a kneaded product obtained by kneading under specific kneading conditions, and the Mv satisfy the following relationship: “{Mv−Mv(A)}/Mv is 0.20 or less”, and the ultrahigh-molecular-weight polyethylene powder contains an ultrahigh-molecular-weight polyethylene powder having a particle size of 212 μm or larger, wherein the powder having a particle size of 212 μm or larger has an average pore volume of 0.6 ml/g or larger and an average pore size of 0.3 μm or larger.",
  "title": "Ultrahigh-Molecular-Weight Polyethylene Powder"
}