  "description": "The present invention relates to a method for activating a secondary battery. The present invention comprises: a primary charging step of charging a secondary battery including a positive electrode, a negative electrode, a separator, and an electrolyte; a room temperature-aging step of storing, at…",
  "path": "/patents/1427757",
  "publishedAt": "2023-04-12T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/04",
    "LG CHEMICAL LTD [KR]"
  ],
  "textContent": "The present invention relates to a method for activating a secondary battery. The present invention comprises: a primary charging step of charging a secondary battery including a positive electrode, a negative electrode, a separator, and an electrolyte; a room temperature-aging step of storing, at a room temperature, the secondary battery that has undergone the primary charging step; and a high temperature-aging step of storing, at a high temperature, the secondary battery that has undergone the room temperature-aging step, wherein charging/discharging is performed by alternately applying + current and - current to the secondary battery at the end of the primary charging step. The method for activating a secondary battery according to the present invention includes alternately applying + current and - current to the secondary battery at the end of the primary charging step to stabilize an SEI film, thereby shortening a following-up aging time.",
  "title": "METHOD FOR ACTIVATING SECONDARY BATTERY"
}