  "$type": "site.standard.document",
  "description": "A lithium ion battery manufacturing method comprising: a step for forming a PGLYD polymer imparted with adhesiveness by forming a urethane bond on a PGLYD polymer; a step for forming a positive electrode containing lithium, iron, phosphorus, and amorphous carbon; a step for forming a negative…",
  "path": "/patents/1427350",
  "publishedAt": "2026-06-24T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/13",
    "NASH ENERGY I PRIVATE LTD [IN]"
  ],
  "textContent": "A lithium ion battery manufacturing method comprising: a step for forming a PGLYD polymer imparted with adhesiveness by forming a urethane bond on a PGLYD polymer; a step for forming a positive electrode containing lithium, iron, phosphorus, and amorphous carbon; a step for forming a negative electrode containing graphite and amorphous carbon; and a step for placing the positive electrode, the negative electrode, and a predetermined electrolyte in a predetermined container and sealing the container, wherein at least one of the positive electrode and the negative electrode comprises the PGLYD polymer imparted with adhesiveness as a binder.",
  "title": "LITHIUM ION BATTERY AND LITHIUM ION BATTERY MANUFACTURING METHOD"
}