"$type": "site.standard.document",
"coverImage": {
"$type": "blob",
"ref": {
"$link": "bafkreifmqk7pgrkvfdgsydei6m44gfg4buewidyoynlg4tr4qxbc4urd5i"
},
"mimeType": "image/png",
"size": 108308
},
"description": "The invention is intended to provide a technology for maintain surface unevenness of a decorative film for film insert molding. [0002] The present invention provides a decorative film for film insert molding, the decorative film having: a fluorine-based resin layer containing 100 to 80 parts by…",
"path": "/patents/1424785",
"publishedAt": "2024-04-24T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B29C45/14",
"DENKA COMPANY LTD [JP]"
],
"textContent": "The invention is intended to provide a technology for maintain surface unevenness of a decorative film for film insert molding. [0002] The present invention provides a decorative film for film insert molding, the decorative film having: a fluorine-based resin layer containing 100 to 80 parts by mass of a fluorine-based resin and 0 to 20 parts by mass of a methacrylic acid ester-based resin; an acrylic-based resin layer containing 50 to 0 parts by mass of a fluorine-based resin and 50 to 100 parts by mass of a methacrylic acid ester-based resin; and a decorative layer containing a thermoplastic resin, laminated therein in this order, wherein the fluorine-based resin layer has a thickness of 10 µm to 200 µm, and surface unevenness is formed on a surface of the fluorine-based resin layer, the surface being on the side that is not in contact with the acrylic-based resin layer. The present invention also provides a method for manufacturing the decorative film for film insert molding.",
"title": "DECORATIVE FILM FOR FILM INSERT MOLDING AND METHOD FOR MANUFACTURING SAME"
}