"description": "A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to…",
"path": "/patents/1284372",
"publishedAt": "2021-02-25T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/525",
"BASF SE"
],
"textContent": "A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to 2000° C., wherein TM contains nickel and at least one further transition metal selected from cobalt and manganese.",
"title": "PROCESS FOR MAKING A MIXED METAL OXIDE"
}