"description": "A method of making an interconnect for a solid oxide fuel cell stack includes contacting an interconnect powder located in a die cavity with iron, the interconnect powder including a chromium and iron, compressing the interconnect powder to form an interconnect having ribs and fuel channels on a…",
"path": "/patents/1285592",
"publishedAt": "2021-03-11T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M8/0202",
"BLOOM ENERGY CORPORATION"
],
"textContent": "A method of making an interconnect for a solid oxide fuel cell stack includes contacting an interconnect powder located in a die cavity with iron, the interconnect powder including a chromium and iron, compressing the interconnect powder to form an interconnect having ribs and fuel channels on a first side of the interconnect, such that the iron is disposed on tips of the ribs; and sintering the interconnect, such that the iron forms an contact layer on the tips of the ribs having a higher iron concentration than a remainder of the interconnect. A glass containing cathode contact layer having a glass transition temperature of 900° C. or less may be located over the rib tips on the oxidant side of the interconnect.",
"title": "FUEL CELL INTERCONNECT WITH REDUCED VOLTAGE DEGRADATION AND MANUFACTURING METHOD"
}