  "description": "A process for making a partially coated electrode active material may involve: (a) providing an electrode active material of the formula LiTMO, wherein TM is a combination of Ni, Co and, optionally, Mn, and, optionally, at least one metal selected from Al, Ti, Mo, W, and Zr, and x is in the range…",
  "path": "/patents/1286196",
  "publishedAt": "2021-03-18T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/525",
    "BASF SE"
  ],
  "textContent": "A process for making a partially coated electrode active material may involve: (a) providing an electrode active material of the formula LiTMO, wherein TM is a combination of Ni, Co and, optionally, Mn, and, optionally, at least one metal selected from Al, Ti, Mo, W, and Zr, and x is in the range of from zero to 0.2, wherein at least 60 mole-% of the transition metal of TM is Ni, and wherein the electrode active material has a residual moisture content in the range of from 50 to 1,000 ppm; (b) treating the electrode active material with a metal alkoxide or metal halide or metal amide or alkyl metal compound; (c) treating the material obtained in (b) with moisture; and (d) repeating the sequence of (b) and (c) twice to 4 times, wherein, in the last sequence of (b) and (c), moisture is at least partially substituted by ozone.",
  "title": "PROCESS FOR MAKING A PARTIALLY COATED ELECTRODE ACTIVE MATERIAL, AND ELECTRODE ACTIVE MATERIAL"
}