NEGATIVE ELECTRODE FOR POWER STORAGE DEVICE, AND POWER STORAGE DEVICE

DRIVE June 17, 2026
Source
A negative electrode (22) for a power storage device includes a negative electrode current collector (22a) including a first surface (22a1), and a negative electrode active material layer (22b) formed on the first surface (22a1) of the negative electrode current collector (22a). The weight per unit area of the negative electrode active material layer (22b) is 20 mg/cm2 or greater. The negative electrode active material layer (22b) contains graphite, an aqueous binder having a glass transition temperature less than 7°C, and single-walled carbon nanotubes.