"$type": "site.standard.document",
"description": "A crosslinked polyolefin separator having an average value of light transmittance of 30% or more in a region of 380 nm to 700 nm, after four sides of the separator are fixed and allowed to stand at 130° C. for 30 minutes. A method for manufacturing the crosslinked polyolefin separator is also…",
"path": "/patents/1296532",
"publishedAt": "2021-07-29T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M50/417",
"LG Chem, Ltd."
],
"textContent": "A crosslinked polyolefin separator having an average value of light transmittance of 30% or more in a region of 380 nm to 700 nm, after four sides of the separator are fixed and allowed to stand at 130° C. for 30 minutes. A method for manufacturing the crosslinked polyolefin separator is also provided. The crosslinked polyolefin separator has a low shutdown temperature to provide improved safety. The crosslinked polyolefin separator also has a high meltdown temperature and is inhibited from die-drooling.",
"title": "Cross-Linked Polyolefin Separator and Method for Producing Same"
}