"$type": "site.standard.document",
"description": "A glass frit includes a glass which contains: Li; at least one selected from the group consisting of B, Si, P, Ge, and Te; O; and at least one selected from the group consisting of F, Cl, Br, and I. The glass is to turn into a crystallized glass including an amorphous phase and a crystalline phase…",
"path": "/patents/1297533",
"publishedAt": "2021-08-12T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/0562",
"AGC Inc."
],
"textContent": "A glass frit includes a glass which contains: Li; at least one selected from the group consisting of B, Si, P, Ge, and Te; O; and at least one selected from the group consisting of F, Cl, Br, and I. The glass is to turn into a crystallized glass including an amorphous phase and a crystalline phase, the crystalline phase precipitated by a heat treatment at a temperature equal to or higher than a glass transition temperature and equal to or lower than a glass crystallization temperature. The crystallized glass shows diffraction peaks at 2θ=22.8±0.5°, 2θ=32.1±0.5° and 2θ=39.6±0.5° in a powder X-ray diffraction pattern using Cu—Kα radiation.",
"title": "GLASS FRIT, CRYSTALLIZED GLASS, METHOD FOR PRODUCING CRYSTALLIZED GLASS, SOLID ELECTROLYTE, AND LITHIUM ION SECONDARY BATTERY"
}