  "description": "A lithium-metal battery, includes: a substrate; a cathode disposed on the substrate; a garnet solid-state electrolyte disposed on the cathode; and a lithium anode disposed on the garnet solid-state electrolyte, such that a discoloration layer is disposed at an interface of the lithium anode and…",
  "path": "/patents/1300152",
  "publishedAt": "2021-09-16T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0585",
    "Corning Incorporated"
  ],
  "textContent": "A lithium-metal battery, includes: a substrate; a cathode disposed on the substrate; a garnet solid-state electrolyte disposed on the cathode; and a lithium anode disposed on the garnet solid-state electrolyte, such that a discoloration layer is disposed at an interface of the lithium anode and garnet solid-state electrolyte, the discoloration layer includes: a first portion; and a second portion, such that the first portion has a lithium component and the second portion has a garnet component. A method of forming a lithium-metal battery, includes: stacking a garnet source with at least one lithium source; and heating the stack at a temperature of at least 300° C. for a time in a range of 1 sec to 20 min to form a discoloration layer, such that the discoloration layer is disposed at an interface of the garnet source and the lithium source.",
  "title": "LI/GARNET ELECTROLYTE INTERFACE WITH LOW INTERFACIAL RESISTANCE"
}