"description": "A method for producing a sulfide solid electrolyte, comprising a firing step of firing a raw material containing Li2S in a hydrogen sulfide-containing atmosphere at a temperature of 300°C or higher, Li2S having a purity of 50 to 90% by mass at the start of firing. Li2S may contain impurities…",
"path": "/patents/1412864",
"publishedAt": "2024-05-01T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C01B17/22",
"MITSUI MINING & SMELTING CO LTD [JP]"
],
"textContent": "A method for producing a sulfide solid electrolyte, comprising a firing step of firing a raw material containing Li2S in a hydrogen sulfide-containing atmosphere at a temperature of 300°C or higher, Li2S having a purity of 50 to 90% by mass at the start of firing. Li2S may contain impurities including at least one of LiOH, Li2O, LiHCO3, and Li2CO3. In the firing step, it is preferable that a concentration of a hydrogen sulfide in the hydrogen sulfide-containing atmosphere is 50 volume% or more. It is preferable that the raw material further contains P2S5 and LiX (X represents at least one type of elemental halogen), and the sulfide solid electrolyte has an argyrodite-type crystal structure.",
"title": "METHOD FOR PRODUCING SULFIDE SOLID ELECTROLYTE"
}