  "description": "Provided is an acrylic resin layer laminate having excellent impact resistance and smaller fragments generated at the time of impact. The laminate includes a first acrylic resin layer, a thermoplastic resin layer, and a second acrylic resin layer in this order, in which a ratio [T:T] of a thickness…",
  "path": "/patents/1412677",
  "publishedAt": "2024-03-13T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B29C45/0001",
    "SUMITOMO CHEMICAL CO [JP]"
  ],
  "textContent": "Provided is an acrylic resin layer laminate having excellent impact resistance and smaller fragments generated at the time of impact. The laminate includes a first acrylic resin layer, a thermoplastic resin layer, and a second acrylic resin layer in this order, in which a ratio [T:T] of a thickness T of the first acrylic resin layer to a thickness T of the second acrylic resin layer is within a range of 1:1.9 to 1:29, and the second acrylic resin layer is formed of a (meth)acrylic resin having a Vicat softening temperature of 115°C or higher and 145°C or lower.",
  "title": "LAMINATE AND MANUFACTURING METHOD OF A LAMINATE"
}