  "$type": "site.standard.document",
  "description": "Provided are an acrylic resin layer laminate having excellent impact resistance and a manufacturing method of the same. The laminate includes a first acrylic resin layer, a thermoplastic resin layer, and a second acrylic resin layer in this order, in which the thermoplastic resin layer contains 71%…",
  "path": "/patents/1412690",
  "publishedAt": "2024-03-13T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B32B27/08",
    "SUMITOMO CHEMICAL CO [JP]"
  ],
  "textContent": "Provided are an acrylic resin layer laminate having excellent impact resistance and a manufacturing method of the same. The laminate includes a first acrylic resin layer, a thermoplastic resin layer, and a second acrylic resin layer in this order, in which the thermoplastic resin layer contains 71% or more of a component having a spin-spin relaxation time T2H in pulse NMR measurement of 0.03 ms or longer. The manufacturing method of the laminate includes: discharging, from a die, a molten resin laminate containing at least a melt of a resin composition (1) containing a (meth)acrylic resin, a melt of a resin composition containing a thermoplastic resin, and a melt of a resin composition (2) containing a (meth)acrylic resin; and cooling the discharged molten resin laminate to obtain a laminate.",
  "title": "LAMINATE AND MANUFACTURING METHOD OF A LAMINATE"
}