  "$type": "site.standard.document",
  "description": "The present invention relates to a method for producing an electrolytic copper foil, the method enabling providing an electrolytic copper foil such that the electrical conductivity is 99% or more, the thickness is 10 μm or less, a problem of a bend is suppressed, the front side and the rear side…",
  "path": "/patents/1302209",
  "publishedAt": "2021-10-14T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C25D3/38",
    "TEX TECHNOLOGY INC."
  ],
  "textContent": "The present invention relates to a method for producing an electrolytic copper foil, the method enabling providing an electrolytic copper foil such that the electrical conductivity is 99% or more, the thickness is 10 μm or less, a problem of a bend is suppressed, the front side and the rear side are flat, the tensile strength is 500 MPa or more, and the elongation percentage is 5.5% or more. The method for producing an electrolytic copper foil includes forming an electrolytic copper foil by using, as an electrolytic solution, a sulfuric acid-copper sulfate aqueous solution not containing a heavy metal other than a copper metal, using an insoluble anode and a cathode drum facing the insoluble anode, and passing a direct current between these electrodes, wherein, in the electrolytic solution, particular additives (A) to (E) are contained each in a particular amount, and the additive (D) and the additive (A) are each added in a ratio such that (D)/(A) is 0.2 to 0.7.",
  "title": "METHOD FOR PRODUCING ELECTROLYTIC COPPER FOIL"
}