METHOD FOR ANAEROBICALLY CRACKING POWER BATTERY
DRIVE
December 9, 2021
Disclosed is a method for anaerobically cracking a power battery, which includes the following steps: disassembling a waste power battery to obtain a battery cell; taking out a diaphragm from the battery cell for later use, and pyrolyzing the battery cell to obtain electrode powder; extracting nickel, cobalt and manganese elements from the electrode powder with an extraction buffer, filtering, taking the filtrate, then adjusting the filtrate with a nickel solution, a cobalt solution and a manganese solution to obtain a solution A, adding the solution A dropwise into ammonium hydroxide under stirring, and then adding an alkali solution under stirring to obtain a solution B; subjecting the solution B to a hydrothermal reaction, filtering, and roasting to obtain a catalyst, such that a chemical formula of the catalyst is NiCoMnO, where 0.25≤x