  "$type": "site.standard.document",
  "description": "A cathode active material for a lithium secondary battery including a lithium-transition metal composite oxide particle is provided. A crystal grain size of the lithium-transition metal composite oxide particle measured by an XRD analysis is 250 nm or more, and an XRD peak intensity ratio of the…",
  "path": "/patents/1306133",
  "publishedAt": "2021-12-09T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/525",
    "SK INNOVATION CO., LTD."
  ],
  "textContent": "A cathode active material for a lithium secondary battery including a lithium-transition metal composite oxide particle is provided. A crystal grain size of the lithium-transition metal composite oxide particle measured by an XRD analysis is 250 nm or more, and an XRD peak intensity ratio of the lithium-transition metal composite oxide particle is 9.8% or less. A lithium secondary battery including the lithium-transition metal composite oxide particle and having improved life-span and rate capability is provided.",
  "title": "CATHODE ACTIVE MATERIAL FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY INCLUDING THE SAME"
}