  "description": "A method for producing a metal composite hydroxide, which includes a first crystallization process of supplying a first raw material aqueous and performing a crystallization reaction and a second crystallization process of supplying a second raw material aqueous solution containing a more amount of…",
  "path": "/patents/1306930",
  "publishedAt": "2021-12-23T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01G53/04",
    "SUMITOMO METAL MINING CO., LTD."
  ],
  "textContent": "A method for producing a metal composite hydroxide, which includes a first crystallization process of supplying a first raw material aqueous and performing a crystallization reaction and a second crystallization process of supplying a second raw material aqueous solution containing a more amount of tungsten than the first raw material aqueous solution and performing a crystallization reaction to form a tungsten-concentrated layer and in which switching of reaction atmosphere from either atmosphere of a non-oxidizing atmosphere or an oxidizing atmosphere to the other atmosphere is performed two or more times in particle growth and the time for supplying the second raw material aqueous solution into the reaction tank in the non-oxidizing atmosphere is 50% or more with respect to the entire time for supplying the second raw material aqueous solution into the reaction tank.",
  "title": "METAL COMPOSITE HYDROXIDE AND METHOD FOR PRODUCING THE SAME, POSITIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY AND METHOD FOR PRODUCING THE SAME, AND LITHIUM ION SECONDARY BATTERY USING THE SAME"
}