  "description": "The conjugated diene-based polymer has a Mooney viscosity measured at 100°C of 40 or more and 170 or less, has Mooney stress relaxation measured at 100°C of 0.35 or less, and has a branch number (Bn) measured by viscosity detector-equipped GPC-light scattering measurement of 8 or more.",
  "path": "/patents/1408738",
  "publishedAt": "2024-09-04T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B60C1/00",
    "ASAHI CHEMICAL IND [JP]"
  ],
  "textContent": "The conjugated diene-based polymer has a Mooney viscosity measured at 100°C of 40 or more and 170 or less, has Mooney stress relaxation measured at 100°C of 0.35 or less, and has a branch number (Bn) measured by viscosity detector-equipped GPC-light scattering measurement of 8 or more.",
  "title": "CONJUGATED DIENE POLYMER, METHOD FOR PRODUCING CONJUGATED DIENE POLYMER, CONJUGATED DIENE POLYMER COMPOSITION, AND RUBBER COMPOSITION"
}