  "$type": "site.standard.document",
  "description": "A sulfide solid electrolyte has peak A at 2θ = 20.7° ± 0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKal radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ = 25.4° ± 1.0° in the X-ray diffraction pattern obtained by…",
  "path": "/patents/1408588",
  "publishedAt": "2024-02-28T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01B17/22",
    "MITSUI MINING & SMELTING CO LTD [JP]"
  ],
  "textContent": "A sulfide solid electrolyte has peak A at 2θ = 20.7° ± 0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKal radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ = 25.4° ± 1.0° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKal radiation. It is also preferable that the value of the ratio of IA to IB, IA/IB, is more than 0 and 0.7 or less, where IA is the intensity of peak A and IB is the intensity of peak B. It is also preferable that the sulfide solid electrolyte has peak C at 2θ = 22.0° ± 0.5° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKal radiation.",
  "title": "SULFIDE SOLID ELECTROLYTE"
}