"description": "An electrode structure includes a positive electrode layer and a positive electrode collector member. The positive electrode collector member includes a positive electrode collector foil, a carbon film, and a hot melt adhesive agent. A positive electrode total specific surface area is more than or…",
"path": "/patents/1308148",
"publishedAt": "2022-01-06T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/667",
"Toyota Jidosha Kabushiki Kaisha"
],
"textContent": "An electrode structure includes a positive electrode layer and a positive electrode collector member. The positive electrode collector member includes a positive electrode collector foil, a carbon film, and a hot melt adhesive agent. A positive electrode total specific surface area is more than or equal to 2.2 m/g and less than or equal to 3.0 m/g, the positive electrode total specific surface area being represented by a total of a product of weight ratio and specific surface area of a positive electrode active material, a product of weight ratio and specific surface area of a solid electrolyte, and a product of weight ratio and specific surface area of a conductive material. A softening point of the hot melt adhesive agent is more than or equal to 100° C. and less than or equal to 130° C.",
"title": "ELECTRODE STRUCTURE"
}