"description": "A method for producing a lithium-containing composite oxide, the method including: a first step of preparing a lithium hydroxide; a second step of heating a hydroxide containing nickel and a metal M1 other than lithium and nickel to 300° C. or higher and 800° C. or lower, to obtain a composite…",
"path": "/patents/1311633",
"publishedAt": "2022-02-24T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/525",
"Panasonic Intellectual Property Management Co., Ltd."
],
"textContent": "A method for producing a lithium-containing composite oxide, the method including: a first step of preparing a lithium hydroxide; a second step of heating a hydroxide containing nickel and a metal M1 other than lithium and nickel to 300° C. or higher and 800° C. or lower, to obtain a composite oxide containing the nickel and the metal M; a third step of mixing the lithium hydroxide and the composite oxide, to obtain a mixture; a fourth step of compression-molding the mixture, to obtain a molded body; and a fifth step of baking the molded body at 600° C. or higher and 850° C. or lower, to obtain a baked body.",
"title": "LITHIUM-CONTAINING COMPLEX OXIDE PRODUCTION METHOD"
}