"description": "A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio D/Dof a 90% particle size Dto a 10% particle size Din volume-based cumulative particle sizeā¦",
"path": "/patents/1314410",
"publishedAt": "2022-03-31T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/505",
"Nichia Corporation"
],
"textContent": "A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio D/Dof a 90% particle size Dto a 10% particle size Din volume-based cumulative particle size distribution is 3 or less; mixing the composite oxide particles and a lithium compound to obtain a first mixture; subjecting the first mixture to a first heat treatment at a first temperature and a second heat treatment at a second temperature higher than the first temperature to obtain a first heat-treated product; and subjecting the first heat-treated material to a dispersion treatment.",
"title": "METHOD OF PRODUCING POSITIVE ELECTRODE ACTIVE MATERIAL FOR NONAQUEOUS ELECTROLYTE SECONDARY BATTERY"
}