"description": "A method for producing a positive electrode active material for a non-aqueous electrolyte secondary battery. The method includes providing a composition containing a first lithium transition metal composite oxide having a 50% particle size Din a first volume cumulative particle size distribution of…",
"path": "/patents/1314413",
"publishedAt": "2022-03-31T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/525",
"NICHIA CORPORATION"
],
"textContent": "A method for producing a positive electrode active material for a non-aqueous electrolyte secondary battery. The method includes providing a composition containing a first lithium transition metal composite oxide having a 50% particle size Din a first volume cumulative particle size distribution of 0.1 μm or more and less than 3.2 μm and a first liquid medium; and granulating the composition to obtain a second lithium transition metal composite oxide having a 50% particle size Din a second volume cumulative particle size distribution greater than D. The second lithium transition metal composite oxide has a ratio of a 90% particle size Din a third volume cumulative particle size distribution measured after the ultrasonic treatment to a 90% particle size Din the second volume cumulative particle size distribution measured before the ultrasonic treatment (D/D) of 0.53 or less.",
"title": "POSITIVE ELECTRODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY, AND METHOD FOR PRODUCING SAME"
}