"$type": "site.standard.document",
"description": "An electrolytic copper foil having higher electrical conductivity, and a method for producing the same are provided. The electrolytic copper foil according the present invention has a carbon content of 5 ppm or less, a sulfur content of 3 ppm or less, an oxygen content of 5 ppm or less, and a…",
"path": "/patents/1315197",
"publishedAt": "2022-04-14T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C25D1/04",
"NIPPON DENKAI, LTD."
],
"textContent": "An electrolytic copper foil having higher electrical conductivity, and a method for producing the same are provided. The electrolytic copper foil according the present invention has a carbon content of 5 ppm or less, a sulfur content of 3 ppm or less, an oxygen content of 5 ppm or less, and a nitrogen content of 0.5 ppm or less; has a total content of carbon, sulfur, oxygen, nitrogen, and hydrogen of 15 ppm or less; and has a number of grains of 8.0 to 12.0/μm, the number of grains changing to 0.6 to 1.0/μmby heating the electrolytic copper foil at 150° C. for 1 hour. A method for producing this electrolytic copper foil includes cleaning a copper raw material; dissolving the copper raw material after the cleaning to obtain an electrolytic solution having a total organic carbon (TOC) of 10 ppm or less; and electrolyzing the electrolytic solution to obtain the electrolytic copper foil.",
"title": "ELECTROLYTIC COPPER FOIL AND METHOD FOR PRODUCING SAME"
}