"$type": "site.standard.document",
"description": "The present invention relates to a method for manufacturing an electrode for a lithium secondary battery, wherein, at the time of manufacturing of an electrode for a lithium secondary battery, a drying speed can be reduced through the steps of: applying a dewatering process using a porous substrate…",
"path": "/patents/1403443",
"publishedAt": "2026-04-08T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/052",
"SEOUL NAT UNIV R&DB FOUNDATION [KR]"
],
"textContent": "The present invention relates to a method for manufacturing an electrode for a lithium secondary battery, wherein, at the time of manufacturing of an electrode for a lithium secondary battery, a drying speed can be reduced through the steps of: applying a dewatering process using a porous substrate to remove a considerable amount of solvent from electrode slurry in advance; performing pressurization in a state of the porous substrate, an electrode layer, and an electrode current collector; performing additional dewatering; and separating the porous substrate from the electrode layer and then drying the electrode layer, and thus the electrode productivity can be maximized without degradation of electrode performance.",
"title": "METHOD FOR MANUFACTURING ELECTRODE FOR LITHIUM SECONDARY BATTERY"
}