  "$type": "site.standard.document",
  "description": "A method for forming a positive electrode active material of a lithium ion secondary battery is provided. In the method for forming a positive electrode active material, a first container that includes a mixture of lithium oxide, fluoride, and a magnesium compound and fluoride that is outside the…",
  "path": "/patents/1320325",
  "publishedAt": "2022-06-16T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/525",
    "SEMICONDUCTOR ENERGY LABORATORY CO., LTD."
  ],
  "textContent": "A method for forming a positive electrode active material of a lithium ion secondary battery is provided. In the method for forming a positive electrode active material, a first container that includes a mixture of lithium oxide, fluoride, and a magnesium compound and fluoride that is outside the first container are provided in a heating furnace, and the heating furnace is heated at a temperature higher than or equal to a temperature at which the fluoride is volatilized or sublimated. It is further preferable that the fluoride be lithium fluoride and the magnesium compound be magnesium fluoride.",
  "title": "METHOD FOR FORMING POSITIVE ELECTRODE ACTIVE MATERIAL"
}