"$type": "site.standard.document",
"description": "Disclosed is a method for manufacturing a dry electrode. The method allows determination of the micro-fibrilization degree of a binder resin from the crystallinity of the binder resin. Based on this, the processing conditions of mixed powder for electrode or an electrode film may be controlled. In…",
"path": "/patents/1401380",
"publishedAt": "2025-01-01T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01G11/86",
"LG ENERGY SOLUTION LTD [KR]"
],
"textContent": "Disclosed is a method for manufacturing a dry electrode. The method allows determination of the micro-fibrilization degree of a binder resin from the crystallinity of the binder resin. Based on this, the processing conditions of mixed powder for electrode or an electrode film may be controlled. In this manner, it is possible to check and control the processing conditions easily and efficiently. In addition, the method for manufacturing a dry electrode includes a kneading step using a kneader under a low speed and high temperature and pulverization step. Therefore, there is no problem of blocking of a flow path caused by aggregation of the ingredients, which is favorable to mass production.",
"title": "ELECTRODE FOR ELECTROCHEMICAL DEVICE COMPRISING DRY ELECTRODE FILM AND METHOD FOR MANUFACTURING THE SAME"
}