  "description": "An anode active material for a secondary battery includes an anode current collector, and an anode active material layer formed on the anode current collector and including carbon-based active material particles and a silicon coating formed on surfaces of the carbon-based active material particles…",
  "path": "/patents/1399124",
  "publishedAt": "2024-12-18T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/052",
    "SK ON CO LTD [KR]"
  ],
  "textContent": "An anode active material for a secondary battery includes an anode current collector, and an anode active material layer formed on the anode current collector and including carbon-based active material particles and a silicon coating formed on surfaces of the carbon-based active material particles. A surface content of silicon of the anode active material layer measured by an X-ray photoelectric spectroscopy (XPS) is in a range from 3 atom% to 25 atom%. A peak intensity ratio defined as a ratio of a second peak intensity corresponding to a peak intensity at a binding energy in a range from 102 eV to 106 eV relative to a first peak intensity corresponding to a peak intensity at a binding energy in a range from 98 eV to 102 eV is in a range from 0.05 to 1.",
  "title": "ANODE FOR SECONDARY BATTERY, METHOD OF FABRICATING THE SAME AND LITHIUM SECONDARY BATTERY INCLUDING THE SAME"
}