  "$type": "site.standard.document",
  "description": "A method of recovering cobalt and nickel includes the steps of: adding alkaline to an acidic solution containing aluminum together with cobalt and nickel, adjusting pH of the acidic solution to 5 to 7, and converting the cobalt, the nickel and the aluminum into hydroxides thereof; recovering the…",
  "path": "/patents/1398379",
  "publishedAt": "2025-09-24T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01G51/04",
    "MITSUBISHI MATERIALS CORP [JP]"
  ],
  "textContent": "A method of recovering cobalt and nickel includes the steps of: adding alkaline to an acidic solution containing aluminum together with cobalt and nickel, adjusting pH of the acidic solution to 5 to 7, and converting the cobalt, the nickel and the aluminum into hydroxides thereof; recovering the hydroxides by solid-liquid separation, mixing the recovered hydroxides with an alkaline solution, and leaching aluminum contained in the hydroxides under a liquid condition of pH 8 or more; and recovering a cobalt hydroxide and a nickel hydroxide that aluminum is separated therefrom by solid-separation on a leachate.",
  "title": "METHOD FOR RECOVERING COBALT AND NICKEL"
}