"description": "Methods of making a sintered electrode comprise forming a slurry including 40 wt % to 75 wt % of a powder comprising a chalcogenide and at least one of an alkali metal or an alkaline earth metal, 1 wt % to 10 wt % of a binder, and 30 wt % to 50 wt % of a solvent. Methods include casting the slurry…",
"path": "/patents/1329479",
"publishedAt": "2022-10-13T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/581",
"CORNING INCORPORATED"
],
"textContent": "Methods of making a sintered electrode comprise forming a slurry including 40 wt % to 75 wt % of a powder comprising a chalcogenide and at least one of an alkali metal or an alkaline earth metal, 1 wt % to 10 wt % of a binder, and 30 wt % to 50 wt % of a solvent. Methods include casting the slurry into a green tape. Methods include drying the green tape to form a dried green tape by removing at least a portion of the solvent. The dried green tape includes at most 10 wt % of organic material in the dried green tape. Methods include sintering the dried green tape at a temperature from 500° C. to 1350° C. for no more than 60 minutes to form the sintered electrode.",
"title": "SINTERED ELECTRODES FOR BATTERIES AND METHOD OF PREPARING SAME"
}