"$type": "site.standard.document",
"description": "A method of producing a rechargeable lithium battery cell, the method comprising (a) preparing a liquid electrolyte solution comprising an ion-conducting polymer dispersed in a first liquid solvent and an optional lithium salt dissolved in the first liquid solvent; (b) impregnating the electrolyte…",
"path": "/patents/1329965",
"publishedAt": "2022-10-20T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/0569",
"Global Graphene Group, Inc."
],
"textContent": "A method of producing a rechargeable lithium battery cell, the method comprising (a) preparing a liquid electrolyte solution comprising an ion-conducting polymer dispersed in a first liquid solvent and an optional lithium salt dissolved in the first liquid solvent; (b) impregnating the electrolyte solution into the cathode, the anode, a porous structure of the separator, or the battery cell; (c) removing the first liquid solvent; and (d) impregnating a second liquid solvent, comprising an optional lithium salt dissolved therein, into the cathode, the anode, the separator porous structure, or the battery cell; wherein the ion-conducting polymer comprises a polymer having an ion conductivity from 10S/cm to 10S/cm when measured at room temperature without the presence of a liquid solvent and the polymer does not occupy more than 25% by weight of the cathode, not counting a current collector weight.",
"title": "METHOD OF PRODUCING FLAME-RESISTANT QUASI-SOLID ELECTROLYTES AND LITHIUM BATTERIES CONTAINING SAME"
}