"description": "An example component of a machine includes a core layer and an outer layer encasing the core layer. The outer layer has a greater carbon concentration and hardness than the core layer. The outer layer may also be compressively stressed, while the core layer may have tensile stress. The stress…",
"path": "/patents/1330725",
"publishedAt": "2022-11-03T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"F02M61/166",
"Caterpillar Inc."
],
"textContent": "An example component of a machine includes a core layer and an outer layer encasing the core layer. The outer layer has a greater carbon concentration and hardness than the core layer. The outer layer may also be compressively stressed, while the core layer may have tensile stress. The stress and/or hardness profile of the component may enhance its resistance to cracking, particularly in applications where the component is impacted by other object and/or operates at elevated temperatures. The component, such as parts of a fuel injector, may be formed by rough forming the component, carburizing the component, quenching the component, subzero processing the component, and then performing a tempering process. The components may have relatively sharp transition from the high carbon outer layer to the lower carbon core layer. Additionally, the components have a relatively high tempering resistance when used in relatively high temperature environments.",
"title": "COMPONENTS FORMED WITH HIGH STRENGTH STEEL"
}