POSITIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY AND LITHIUM ION SECONDARY BATTERY
DRIVE
November 17, 2022
A positive electrode active material includes lithium transition metal-containing composite oxide particles containing an additive element M1 and includes a coating layer formed of a metal composite oxide of Li and a metal element M2 on a part of a surface of the particles. The particles have a d50 of 3.0 to 7.0 μm, a BET specific surface area of 2.0 to 5.0 m/g, a tap density of 1.0 to 2.0 g/cm, and an oil absorption amount of 30 to 60 ml/100 g. For each of a plurality of primary particles having a primary particle size within a range of 0.1 to 1.0 μm among the primary particles, a coefficient of variation of the concentration of M1 is 1.5 or less, and the amount of M2 is 0.1 to 1.5 atom % with respect to the total number of atoms of Ni, Mn, and Co contained in the composite oxide particles.