POSITIVE ELECTRODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY, AND METHOD OF PRODUCING SAME
DRIVE
February 9, 2023
A method of producing a positive electrode for a non-aqueous electrolyte secondary battery, includes: providing a lithium transition metal composite oxide having a layered structure, having a ratio D/Dof 1 or more and 4 or less, and having a certain content of nickel and a certain content of cobalt; bringing the lithium transition metal composite oxide into contact with a cobalt compound to obtain an adhered material; heat-treating the adhered material at a temperature higher than 700° C. and lower than 1100° C. to obtain a heat-treated product; obtaining a positive electrode composition containing the heat-treated product, a conductive auxiliary agent, and a binder; and applying and pressurizing the positive electrode composition onto a collector to form an active material layer having a density of 2.7 g/cmor more and 3.9 g/cmor less on the collector.