  "$type": "site.standard.document",
  "description": "In a method of preparing an immobilized selenium system or body, a selenium — carbon — oxygen mixture is formed. The mixture is then heated to a temperature above the melting temperature of selenium and the heated mixture is then cooled to ambient or room temperature, thereby forming the…",
  "path": "/patents/1347133",
  "publishedAt": "2023-07-06T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/364",
    "II-VI Delaware, Inc."
  ],
  "textContent": "In a method of preparing an immobilized selenium system or body, a selenium — carbon — oxygen mixture is formed. The mixture is then heated to a temperature above the melting temperature of selenium and the heated mixture is then cooled to ambient or room temperature, thereby forming the immobilized selenium system or body.",
  "title": "IMMOBILIZED SELENIUM IN A POROUS CARBON WITH THE PRESENCE OF OXYGEN, A METHOD OF MAKING, AND USES OF IMMOBILIZED SELENIUM IN A RECHARGEABLE BATTERY"
}