"description": "A method for manufacturing an aluminum alloy sheet may include melting aluminum alloy composition containing silicon (Si), iron (Fe), copper (Cu) and manganese (Mn) in weight% on the basis of remainder of aluminum (Al) to make cast alloy having a constant initial thickness; rolling the cast alloy…",
"path": "/patents/1347718",
"publishedAt": "2023-07-20T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B60R13/0243",
"Hyundai Motor Company"
],
"textContent": "A method for manufacturing an aluminum alloy sheet may include melting aluminum alloy composition containing silicon (Si), iron (Fe), copper (Cu) and manganese (Mn) in weight% on the basis of remainder of aluminum (Al) to make cast alloy having a constant initial thickness; rolling the cast alloy to allow the initial thickness to be reduced, whereby the cast alloy is elongated to aluminum alloy sheet; and performing heat treatment on the aluminum alloy sheet.",
"title": "METHOD FOR MANUFACTURING REAL ALUMINUM USING ALUMINUM ALLOY CAPABLE OF BEING APPLIED TO COIL-TO-UNCOIL PROCESS, AND VEHICLE INTERIOR PART"
}