The present disclosure pertains to: polyamide fibers for an airbag which are characterized in that the fiber size thereof is 200-800 dtex, inclusive, and the stress retention rate thereof when obtained using a prescribed procedure is at least 3.0%; and a method for producing said polyamide fibers for an airbag, the method being characterized in that during the thermosetting step and the relaxing step thereof, the contact time between thread and a roller which is at least 190° C. is at least 30 msec and less than 110 msec, the temperature of the thermosetting roller is 190-205° C., inclusive, the temperature of the relaxing roller is greater than 100° C. and less than 190° C., and the speed ratio of the relaxing roller to the thermosetting roller satisfies this equation: 1.00