  "$type": "site.standard.document",
  "description": "A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio D/Dof a 90% particle size Dto a 10% particle size Din volume-based cumulative particle size…",
  "path": "/patents/1354004",
  "publishedAt": "2023-11-02T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/505",
    "Nichia Corporation"
  ],
  "textContent": "A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio D/Dof a 90% particle size Dto a 10% particle size Din volume-based cumulative particle size distribution is 3 or less; mixing the composite oxide particles and a lithium compound to obtain a first mixture; subjecting the first mixture to a first heat treatment at a first temperature and a second heat treatment at a second temperature higher than the first temperature to obtain a first heat-treated product; and subjecting the first heat-treated material to a dispersion treatment.",
  "title": "METHOD OF PRODUCING POSITIVE ELECTRODE ACTIVE MATERIAL FOR NONAQUEOUS ELECTROLYTE SECONDARY BATTERY"
}