  "$type": "site.standard.document",
  "description": "A lithium-ion secondary battery includes an inorganic filler having a mean particle size of 1 μm to 10 μm. A ratio A/B is 14 to 28, where A is a weight ratio of a second binder and the inorganic filler (i.e., second binder/inorganic filler) in an insulating layer, and B is a weight ratio of a first…",
  "path": "/patents/1355069",
  "publishedAt": "2023-11-23T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/13",
    "TOYOTA JIDOSHA KABUSHIKI KAISHA"
  ],
  "textContent": "A lithium-ion secondary battery includes an inorganic filler having a mean particle size of 1 μm to 10 μm. A ratio A/B is 14 to 28, where A is a weight ratio of a second binder and the inorganic filler (i.e., second binder/inorganic filler) in an insulating layer, and B is a weight ratio of a first binder and positive electrode active material particles (i.e., first binder/positive electrode active material particles) in a positive electrode active material layer.",
  "title": "NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY"
}