  "$type": "site.standard.document",
  "description": "A method of manufacturing a lithium solid electrolyte, the method including: providing a composition including a lithium precursor, a lanthanum precursor, and a zirconium precursor; disposing the composition on a substrate having a temperature of 270° C. to 500° C. to form a film; and heat-treating…",
  "path": "/patents/1355516",
  "publishedAt": "2023-11-30T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0562",
    "SAMSUNG ELECTRONICS CO., LTD."
  ],
  "textContent": "A method of manufacturing a lithium solid electrolyte, the method including: providing a composition including a lithium precursor, a lanthanum precursor, and a zirconium precursor; disposing the composition on a substrate having a temperature of 270° C. to 500° C. to form a film; and heat-treating the film at 300° C. to less than 750° C. for 1 hour to 100 hours to manufacture the lithium solid electrolyte.",
  "title": "LITHIUM SOLID ELECTROLYTE AND METHOD OF MANUFACTURE THEREOF"
}