"$type": "site.standard.document",
"description": "Described herein is a process for making a particulate (oxy)hydroxide of TM, where TM are metals and TM includes at least 60 mol-% nickel, and where said process includes the steps of:",
"path": "/patents/1356520",
"publishedAt": "2023-12-21T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C01G53/006",
"BASF SE"
],
"textContent": "Described herein is a process for making a particulate (oxy)hydroxide of TM, where TM are metals and TM includes at least 60 mol-% nickel, and where said process includes the steps of:",
"title": "PROCESS FOR MAKING A PARTICULATE (OXY)HYDROXIDE, AND PARTICULATE (OXY)HYDROXIDE AND ITS USE"
}