"$type": "site.standard.document",
"coverImage": {
"$type": "blob",
"ref": {
"$link": "bafkreigq5mph2p34buis7u6ysgszt52qjtdagfaeufedmrkfl4ub6bx77e"
},
"mimeType": "image/png",
"size": 118480
},
"description": "Provided is an ultrahigh-molecular-weight polyethylene powder having a viscosity-average molecular weight (Mv) of 10×10or higher and 1000×10or lower, having a difference of 3° C. or more between a swelling onset temperature and a dissolution onset temperature determined by a specific method, and…",
"path": "/patents/1357338",
"publishedAt": "2024-01-04T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C08F110/02",
"Asahi Kasei Kabushiki Kaisha"
],
"textContent": "Provided is an ultrahigh-molecular-weight polyethylene powder having a viscosity-average molecular weight (Mv) of 10×10or higher and 1000×10or lower, having a difference of 3° C. or more between a swelling onset temperature and a dissolution onset temperature determined by a specific method, and having a rate of impregnation with liquid paraffin (rate of increase in weight) of 0.5% or more and 5.0% or less determined by a specific method.",
"title": "Ultrahigh-Molecular-Weight Polyethylene Powder and Molded Article Prepared by Molding the Same"
}