"$type": "site.standard.document",
"description": "Disclosed are a method of manufacturing an electrode for secondary batteries that includes surface-treating a current collector so as to have a morphology wherein a surface roughness Rof 0.001 µm to 10 µm is formed over the entire surface thereof, wherein the surface-treating is performed by…",
"path": "/patents/967473",
"publishedAt": "2014-11-12T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/052",
"LG CHEMICAL LTD [KR]"
],
"textContent": "Disclosed are a method of manufacturing an electrode for secondary batteries that includes surface-treating a current collector so as to have a morphology wherein a surface roughness Rof 0.001 µm to 10 µm is formed over the entire surface thereof, wherein the surface-treating is performed by chemical or electrical etching using a wet method or by reactive gas or ion etching using a dry method to enhance adhesion between an electrode active material and the current collector and an electrode for secondary batteries that is manufactured using the method.",
"title": "METHOD FOR MANUFACTURING ELECTRODE FOR LITHIUM SECONDARY BATTERY AND ELECTRODE MANUFACTURED BY USING SAME"
}